Hi All
Just a quick question.
I bought a Mould making starter kit about a year ago.
I have just got round to using it and have opened the mould putty to have a look and it seems to have been overfilled meaning the container hasn't been fully closed and the putty seems quite dry.
Is it still ok to use (i dont want to waste my time if its not going to work) or should I decant it into another container to see how dry it is?
Id rather not have to buy another kit at the moment as money is rather tight,
Any advice would be appreicated.
Cheers guys
Dan
By ajb100
-
1/21/2013 7:47:00 PM
The putty is pretty dry in the container, I use a piece of metal to break the chunks apart and scoop out, if I used my hand it broke through the gloves.
It becomes more pliable once activated and warm