By TomDesign - 1/19/2013 4:08:24 PM				
            
                      
            Hello
  guys im thinking 2 days how to stick flanges to these door panels as hot glue falling of easy .. hm any advise? as i always used this way. i can use glue that used for pva flanges but it melts a little both parts and that not good at all any advise?
 
  Parts been sanded to perfect straight finish. now need flanges somehow to attach then resin infusion. ordering on monday from easycomposites i hope for more things in 1 order they give me better price as last gc 50 was pretty nice deal.
 
  
           
		 | 			
		 
	
		
				      		    
		
		
            
            
            By TomDesign - 1/20/2013 4:40:11 PM				
            
                      
            Thanks a lot im going try my best as that mold is first so hard to add flanges.. 
  i keep update if hot glue not hold good maybe i use pvc glue that a little melt both piece but hold like dead catch.
           
		 | 			
		 
	
	
						
		 	
		
	 |