Ok, so the part that I initially made seems ok, but feels like it had a bit of tack left to it on the back side. When it is warmed up it loses its rigidity and becomes extremely flexible. What could I have done wrong for it to be that way?
By matthieutje65 - 1/15/2013 7:42:18 PM

for flat panels and vacuum bagging you dont need a mould, just use a mirror or glass-plate