Molds is it possible to

http://www.talkcomposites.com/Topic4198.aspx

By Daz - 1/10/2013 7:49:55 AM

Fill a mold you intend to infuse from ?
I made a mold of a wing 
When I gel coated it and left over night
The flange had dropped a little and unbeknown to me pulled away from the wing
Can I fill this
It's on the edge prob about 5 mm deep
And quite long
The part is going to be painted
Is it possible to fill with car body filler and infuse from ??
This is the wing and its to the left 
Which has sagged
I suppose the fibreglass wing I moulded from may have sagged a bit when the unimold went off as there quite flimsy ?
By neilb - 1/11/2013 8:27:45 AM

not yet but i'll txt him now