By twissta - 1/10/2013 1:46:01 AM				
            
                      
            Hello Fam, Can the EF 80 flexible  resin be used in the resin infusion process. I have read the information on the page, however it doesn't mentioned one way or other...?
           
		 | 			
		 
	
		
				      		    
		
		
            
            
            By matthieutje65 - 1/10/2013 2:45:10 AM				
            
                      
            there is a post on this forum talking about this, and if I remember, it was very difficult by using standard resin infusion
           
		 | 			
		 
	
	
						
		 	
		
	 |