Talk Composites - The Forum for Advanced Composites

Superstrong?

http://www.talkcomposites.com/Topic415.aspx

By Zekewarg - 1/31/2012 3:24:14 PM

Hi guys!

2 quick ones:

Q1: Is the adheisive normally used for CF the strongest availiable for that material?
You know when you read about some stealthplane that was glued together? Exactly what kind of glue is that? I don´t mean 
to use it for CF, but that glue must be the best possible for that type of material, so what would be the counterpart for CF?

Q2: If you want to make a superstrong laminate structure, like the one used in high performance sportscars, what recipe would you use?
Without pre-preg that is. What laminates, what core and in what order?
By Joe - 2/1/2012 8:50:00 PM

Paul or Matt from the staff said in a previous post that he would use structural polyurethane between two composites, and epoxy to bond composite to metal or aluminium.

If it can help in any way...