Talk Composites - The Forum for Advanced Composites
Home
»
Advanced Composites Forum
»
Resin Infusion
Preparing Test Sample
http://www.talkcomposites.com/Topic40237.aspx
By Gorkem Emetli
-
7/7/2021 12:18:45 PM
Hello Dear Friends,
I try to prepare test specimen and I used
Eosares 201R (3x)
Eosares 201H (2x)
But Ø12 GFRP Rebar specimen failed 500 MPa.
Could you tell me, what is the reasonable resin mixture?
G.EMETLİ