By carbon man - 7/2/2021 6:18:15 AM
Hi, I believe this is a simular product to duratec sunshield which can bond to epoxy well.
Can I use this as a coating over cured xpreg xc110 parts. Let it dry sand it back and then 2k clear coat? Will it bond to the epoxy ok.
|
By Hanaldo - 7/2/2021 11:53:40 AM
Discussed via PM, but for the sake of anyone that stumbles across this thread - Glosscoat no problem over pre-preg, XC110 or other. Great for filling pinholes without having to do a load of sanding. Just prep well with 240 grit first and you're good to go.
|
|