By S B - 3/7/2021 6:24:49 PM
|
By Hanaldo - 3/12/2021 1:29:01 AM
Use flash tape to seal up any holes again.
Potentially bigger issue - did you use any release agent on the acrylic? Epoxy bonds quite readily to acrylic. Without a release agent, you may find it a massive struggle to remove the acrylic.
|
|