By spire - 12/27/2012 10:26:06 AM

I have some of the Vairi preg 200g pre preg carbon fibre. It is stated on your website that it will cure between 80 and 150 degrees c. Is there a chart or graph you can refer me to as I could do with curing at 100 degrees so therefore need to work out the cure time at this temperature. I will be using a vac bag and oven.

Thank you for your help.