By mporta71 - 11/8/2020 5:42:34 AM
Hi, most of the plastic mixing cups I use do not clean very well after use, especially with epoxy. If I leave the resin inside, it becomes brittle and never detaches completely. If I clean it with acetone, over time the plastic becomes dull getting the problem worse. So do you use any strategy not to waste too many mixing cups? I was thinking about using a realease agent but I am worried about contaminating the resin. Also I try to look for silicone mixing cups but found nothing in the usual stores. Ideas?
|
By Warren (Staff) - 11/16/2020 11:15:59 AM
In theory but they would likely be disproportionately expensive. Also silicone has a limited lifespan with resins in them so after 15-20 pulls would start to break up or have resin stick. So I suspect in the long run it would not be any cheaper.
|
|