+x+xLester that's a beautiful process and part! Is the whole part flax or is there some carbon hiding in there?
This one is 100% flax but this perticular one was just to figure out the process and mostly to see if i can make a bladder inflation mould out of composites as i haven't seen that anywhere back when i made it. i was afraid of creep over time as the mould was pressurized for a long time during the curing of the prepregs.
I am still planning on making a ride-able one which will most likely be a hybrid part, but i will make for the bike i am currently making so i need the frame first. was thinking about making a couple youtube videos as well to give some pointers to other guys.
And thanks Hanaldo. Love your work too! Composites a really cool in the sense that it is really accessible and pretty much everyone can make cool stuff with minimal equipment if you are willing to put in the hours.
If you ever make those videos I'd love to see them, that is some really fine work there!