Question about Vac pump /pressure

http://www.talkcomposites.com/Topic3894.aspx

By fiberpro - 12/18/2012 10:43:01 PM

Hello guys, can someone point me with this problem.

On my vacuum pump is written something like this:




"enddruck"/"ultimate vacuum"  = 150mBar

What doest it mean, how its to 30HG or -1 BAR ?




anyone know?

When i check pump with gauge its shows -0,2 bar.. SO im not sure if this is max of this pump and 150mBar means equal 0,2BAR or pump is broken..

sorry for my english




Regards
By matthieutje65 - 12/19/2012 2:40:28 AM

If I'm correct mBar goes from 0 (full vacuum) till atmospheric pressure (1040-1070)

this means you can achieve a +/- 87,5% vacuum.

Correct me if I'm wrong Smile