By torstenker - 10/5/2020 1:18:49 PM
Hi I have done a lot of testing in the past 3 weeks using all sorts of material combination to test rigidity, weight, resin usage and so on The best 2 samples were with EasyCell75 and 3D Core
Easycell is PVC foam, so I guess I can join sheets with Solvent Cement or similar used for PVC pipes. What can I use to join the 3D PET Core? I'm infusing and the gabs between sheets are visible thanks
|
By Warren (Staff) - 10/5/2020 2:35:16 PM
Yes as said you can epoxy bond it. Or if the mould is a stable shape, just butt join the pieces of 3D core with the hexagons helping to ensure it stays where it is.
|
|