By mikew - 12/12/2012 11:03:20 AM

I'm  making something similar to this

http://www.rally-raidproducts.co.uk/image/cache/data/068-250x250.jpg
which holds this

http://www.f2r.pt/WebRoot/Store/Shops/f2r/4F71/7B12/1C70/C736/82B1/AC10/083A/98C3/RB750-2.JPG

So I need to take a mould off the back of the unit above to get the profile.  It needs to be a snug fit in the holder and I'm wondering what thickness of wax sheet would be best to get the profile correct, 2 mil or 5?

Also when the wax sheet is on, I've seen that some put packing tape over it to prevent sticking, is that a definite method because surely it means sanding work on the mould to remove any lines caused by the tape?
By mikew - 12/16/2012 2:37:47 PM

Cheers both. Using unimould system to make the moould then caron kevlar/epoxy/soric/ply/bag