By Rich in Vancouver - 12/12/2012 6:13:06 AM
Hello, This is my first post and of course it is a newby question.
I am hoping to skin a part made of ABS plastic and would rather not have it melt into
a shapeless blob. Would the black skinning basecoat be safe to use on ABS?
Cheers,
Rich
Vancouver Canada
|
By Rich in Vancouver - 12/12/2012 2:46:09 PM
Thanks for the information Matt. The surface is already textured so rather than smooth it as I
originally intended I will key it instead.
Worse comes to worst I will take a mould from the part and make a proper carbon fibre copy.
(Which would be a better solution just a bit more involved!)
|
|