I'm getting all my stuff tomorrow my scale.
any tips on making moulds
I am using oil-based clay as a fuller is there a better way to make moulds for this part?
hello, do I need to degas tooling Gelcoat in the vacuum degassing chamber? anybody? It would help me to know I am going to start tomorrow.
applying wax, sorry fan is loud
I hope my math is correct. 200grams to 3 grams of harder?
Degassing gelcoat
ok, my math was not right for 100 grams of Gelcoat how much harder di I need in grams ?