By Vanns - 8/29/2020 7:34:47 AM
Hi
Have flattened a board and am going to fill some small cracks with glasscast 3, due to their size i would not need a lot of epoxy...
what kind of curing time am i looking at before i can sand it down?
was going to knock high spots down with a block plane and then orbital.