By thelongride - 8/13/2020 4:59:28 AM
Hello,
I'd like to find a product that results in a fairly porous cured epoxy. The objective being for the cured resin product to absorb (to some degree) liquid paraffin wax. Is anyone aware of a resin system that ends up being (macro)porous? Or and additive that would increase porosity?
Thanks, Pete
|
By oekmont - 8/14/2020 7:31:11 AM
There are foaming additives for epoxys. However, they result in closed porosity.
|
|