+xFor wet layup with woven reinforcement, you use the same weight of resin as you have weight of reinforcement, plus a little bit for wastage. So if your part is 2.5 square metres and you have 2750g (if ive understood that correctly) of fibreglass, then you need 2750g of resin to wet out the fibreglass. You will inevitably waste a bit in the brush or roller and the pot, and maybe be a little resin rich in some areas, so I would probably mix 2850g of resin.
Hi Hanaldo,
Thank you for your response.
I was also thinking the same. However, I could not find any documentation to substantiate the theory.