+x+xHi, it has been a while since I first used Easy-Lease and I cannot remember how it is applied ?? apart from applying at least 6 coats of EL is it buffed in between each coat ?? or not buffed at all, again Thanks Eddie
Hi Eddie, you just wipe it on, wait around 15mins, then wipe on again. Repeating around 6 times on a new mould.
The only time you might do something that could be described as 'buffing' would be when you're applying to glass and you're looking for the best possible surface finish, we sometimes lightly wipe back over a few seconds after the application wipe to break down any smears. This needs to be done very lightly though to avoid accidentally removing the release agent you've just applied. You can find further information on the
Easy-Lease product page and the accompanying technical datasheet.
All the best, Matt
Hi Matt, Thanks again, Regards Eddie