By dougal - 7/17/2020 12:52:40 PM
Hi. I'm interest in peoples experience with adhesives and carbon fibre. I wish to glue a SLS printed part to a carbon fibre tube and a plastic PVC end to the Carbon Fibre. Whats the best adhesive for this?
Kind regards
|
By dougal - 7/17/2020 1:59:17 PM
I believe it is nylon powder that is fused by the SLS process but your recommendation sounds perfect. We will get some sandpaper as well 👍
|
|