By carbon man - 7/11/2020 2:46:51 PM
Is this normal. Every pull seems to add a bit more on. Its on the flange area where there is no carbon laid. But leaves residue of resin. Some flakes off but a lot sticks on?
I put release film over the whole mould surface. 
|
By SleepingAwake - 7/11/2020 10:54:44 PM
Or stick some painters tape on there and it should peel off with the tape.
|
|