By carbon man - 6/28/2020 7:51:45 PM

I see in America they sell partall realese wax designed to stop pva from pooling.

Does anyone know anywhere in the UK that sells this or similar, I can't find anything!

Thanks
By beliblisk - 6/29/2020 5:58:00 PM

carbon man - 6/28/2020 7:51:45 PM
I see in America they sell partall realese wax designed to stop pva from pooling.

Does anyone know anywhere in the UK that sells this or similar, I can't find anything!

Thanks

Easycomposites relese wax works ok for me:

https://www.easycomposites.co.uk/carbon-fibre-skinning-starter-kit

But i spray PVA.