By Barry Marsh - 6/17/2020 11:14:02 PM
I’m brand new to making composites and I’m looking to start out doing some resin infusions and maybe some prepreg down the line.
As I’m new to this hobby I don’t to spend too much money on a vacuum pump as I’m unsure if It’s a hobby I’ll really get into or not.
I had been told by my brother I needed a dual stage pump (I’m assuming he meant for infusions).
I was looking to do quite small jobs. I’m not making boats, probably never do any car sized panels, but a bit smaller.
Do I really need a dual stage pump?
For reference the pump I was looking at was “4.5CFM 2 Stage Refrigerant Vacuum Pump Refrigeration Air Condition 128L/MIN” made by VEVOR.
Any help would be appreciated
|
By Barry Marsh - 6/18/2020 7:15:30 PM
Ok that’s great, thank you and everybody for the advice on this, think I’ll get one of these cheapy pumps.
Does anybody actually use one of these VEVOR pumps?
|
|