By Sentinel Unmanned - 6/9/2020 1:20:45 PM
Is it possible to add further layers of prepreg to a cured part and re-bag & bake?
Will the resins bond ok to the cured parts - I'm assuming the cured part will need keying up?
Thanks in advance
|
By Fasta - 6/11/2020 1:55:14 AM
I do this all the time without film glue. Works great.
|
|