By WaleedMostafa - 6/7/2020 10:15:08 AM
Hi All I need suitable release agent for Acrylic sheet casting of PMMA in glass mold , Facing problem during getting acrylic sheets out from glass mold , Where acrylic sheet is sticking to glass sheets . Could anyone advise me . Thanks in advance
|
By taimur - 6/16/2020 6:40:08 AM
I'm a bit confused regarding all those release agents. ... Number 8 Wax can be used when going from a pattern to a mould or from a ... If you're making flat sheet I would always recommend a glass sheet. ... I'm I right thinking that the first 2 materials would be the best followed by PVC and then perspex?
|
|