Talk Composites - The Forum for Advanced Composites
Home
»
Easy Composites Ltd Technical Support
»
Easy Composites Ltd - Product Specific Pages
»
Carbon Fibre Tube and Section
CF Tube
http://www.talkcomposites.com/Topic3689.aspx
By pedcrist
-
12/6/2012 2:05:38 PM
Hi,
I need to make a 90mm diameter tube and I´m thinking use the 80mm sleeve.
My tube have got to be 1.5/2mm thickness , so my question is: is it easy to apply 3 or 4 sleeves, one above the other, in a pvc mandril?
Pedro
By jay.sun
-
4/14/2017 10:03:50 AM
Hi Matt;
I have lots of carbon fiber tube(braid pultrusion molding).
But, I don't know where need that.
The performance is pretty good. Also I have long tube even more than 3m.
Thank you very much.
JAY