Can anyone tell me the best way to hand lay Carbon Fibre with resin in a mould. I am trying to make a R/C plane, I have already made the mould. I do not have the use of a vacuum pump and wondered if its possible to literally do it by hand with positive results, what are your thoughts?
By dilligaf76 - 5/23/2020 7:43:44 PM

Can you tell me where to get one of these pumps from?