By Neil bickerdike - 5/14/2020 2:01:20 PM				
            
                      
            Hi all I'm Neil from Manchester since being in lock down I have really gotten into carbon skinning etc. So much I have done some interiour parts for friends and done my own car. Looks the nuts. Not perfect but I know were the defaults.  They don't! 😎
  Now I have ordered the vacum pump and starter kit for vaccum bagging etc. Feel I can get a way better finish from this. As well as experimenting with it. 
  Signed for the course as well but seen as we are on lock down and they are putting the finishing touches to the training room, I'm guessing it will become time before I can sharpen my newly acquired hobbie with them
  But I want to say easy compersites the customer service is absolutely awsome. If I need a question answering they answer it via email or if I call. So thankyou to the team. 
           
		 | 			
		 
	
		
				      		    
		
		
            
            
            By Warren (Staff) - 5/15/2020 1:27:58 PM				
            
                      
            Welcome to the forum!  Glad the parts came out nicely!  There is a wealth of experience here on the forum so hopefully you can get any answers you need here.
           
		 | 			
		 
	
	
						
		 	
		
	 |