By Andyx - 4/11/2020 8:14:27 AM
Hi all
Can someone advise best way to make a T shape of carbon fibre hand layering. My current line of thought would be make an L shape and once cured then try and place that on top of a larger section to make the T. Or is it better to make a flat section(the vertical part of the t), trying to keep a section without resin, and later make the T.
Thanks for andy help Andy
|
By Andyx - 4/13/2020 1:02:48 PM
hi, thanks for reply, will get some for next project. thanks again andy
|
|