By Rosta Spicl - 4/3/2020 6:03:41 AM
Dear all Just working on CNC machined mould based on epoxy tooling boad OBO Renshape 5050, which is the similar to Easycomposites EB700. Sanding P600/1000/2000, apply 10+ layers of Frekote FMS, which is the similar to Easycomposites S120, but the surface is still not high gloss, but satin matt. Trying to polish using the cloth, but not shiny like a surface the easycomposites tutorial EB700 shows. Don't you have any tips how polish to high gloss that? Thanks for support Rosta
|
By Rosta Spicl - 4/3/2020 4:58:07 PM
Hanaldo, you right. I was convinced that's the same, but really not. Thx.
|
|