By Mohamed - 3/24/2020 11:50:38 PM
I'm going to use Aluminum honeycomb with density 83 kg/m^3 But i want to run a simulation for my project to make sure that it's being suitable for my project So i want to know the fully properties of the material like (Young's modulus in x,y and z - poisson's ratio in xy,yz,xz - shear modulus in xy,yz,xz -tensile stress and strain in x,y,z -compressive stress and strain in x,y,z - shear stress and strain in xy,yz,xz) to enter it in ansys to run the simulation thanks
|
By Warren (Staff) - 3/30/2020 9:29:57 AM
As oekmont says, that data is not available as it hasn't (and cannot) be measured in the context you are asking for.
|
|