I decided to make some carbon doors for my Noble... unlike the rear clip that was a self made buck to my own design, this time I stripped the original and took moulds of the inner and outer so its effectivelly a replica of the stock part but in carbon....
Also turns out it will be significantly superior as when releasing the moulds from the buck I discovered the standard door edges are made from P40 and filler so the original moulds must have been terrible.
For this part I wanted it strong with some crash protection (unlike original) so on the outer skin I used:
200g carbon
650g carbon
3mm soric
210g Carbon/kevlar
210g Carbon Kevlar
Inside skin hasnt been pulled yet but will not be as heavy as the outer skin so I plan: