By MaxiDave - 11/23/2012 10:45:42 PM				
            
                      
            I'm making a pair of front wings for a car with 300g Kevlar.
  There is one section with a 90 degree bend right, a piece 25-30mm and then a 90 degree bend left
  but I cant get the Kevlar to sit tight on the corners no matter how much I wet it out but when it is half dry/set
  I can mould it into shape pretty good.
  Any advice please? I am doing hand lay up.
           
		 | 			
		 
	
		
				      		    
		
		
            
            
            By MaxiDave - 11/24/2012 8:45:32 PM				
            
                      
            Thanks for the reply.
  How about some of that white plastic corner trim for showers etc, cover it in mould wax and clamp it on?
           
		 | 			
		 
	
	
						
		 	
		
	 |