By Steve B - 2/3/2020 4:43:47 PM				
            
                      
            Hi all, my name is Steve and I work in the maintenance contracting industry using epoxy and polyurethane products to fix industrial tanks, process vessels, bunds, pipework, pumps etc using advanced repair techniques. See www.tlacc.co.uk
  I am an ICorr level 1 coatings inspector.
  When we have slack periods, we make resin tables and plaques - examples below
  
  
  One of the main problems I have encountered making the tables and plaques is controlling the temperature of both the resin and work piece. I now have a solution to this problem – a heated table which can be thermostatically controlled to give me the perfect temperature. It only used 80w power too. Its 1.1m long by .6m wide.
 
  
  I have made 2 of these and put them on ebay https://www.ebay.co.uk/itm/133321710501 - "Heated Table Top with level adjustment and thermostat".  with a full description if anyone is interested. Comments and feedback welcome. 
           
		 | 			
		 
	
		
				      		    
		
		
            
            
            By Warren (Staff) - 2/4/2020 4:53:54 PM				
            
                      
            Sounds like a good idea! Especially for cold workshops.  
           
		 | 			
		 
	
	
						
		 	
		
	 |