By hadi1990 - 1/30/2020 10:10:52 AM

Hello,

I'm making my own carbon fibre frame and iI want to bond the tubes together like the below image.
what type of adhesive do you recommend? 

thx! 

By Warren (Staff) - 1/30/2020 5:29:09 PM

For Structural applications like that, I would recommend our ET515 Semi Flexible 15min Professional Epoxy Adhesive due to its high flexural strength under shock and vibration. 

However, I would NOT recommend a simple butt and fillet joint like in the picture.  You would definitely want a larger surface area and also overlapping fibres or material for strength.  You could wrap the joints with carbon tape or have inserts bonded across the join to strengthen the join.