By Avish - 1/13/2020 4:33:01 PM
Hello, I'm trying to make parts with an outside layer of orange hybrid fabric (by infusion) but when the fabric touches the epoxy- the color is changing immediately to something between dark orange to red... did someone try making orange parts and a found solution to this problem? Maybe there is a diffent type of fabric with lighter orange color? Maybe I should try yellow fabric..? I want exactly the orange color of the fabric before it touches the epoxy. In the picture you can see both dry fabric and final part after curing... Thanks!
|
By Warren (Staff) - 1/16/2020 4:51:10 PM
That almost looks like the red hybrid cloth but photo shades can sometimes be deceiving.
|
|