Talk Composites - The Forum for Advanced Composites
Home
»
Advanced Composites Forum
»
Hand Layup
Achieving 6.3mm thick layup (hand layup, gelcoat, CSM, polyester resin)
http://www.talkcomposites.com/Topic34572.aspx
By JeffKnapman
-
1/13/2020 10:18:37 AM
Need to achieve a 6.3mm thick layup with gelcoat and CSM. What layup schedule would achieve this? Gelcoat + 2x layers of 900gsm CSM?