Hi All, I have a carbon seatpost that has a alloy head attached and I assume is bonded together. The two have since detached and I wondered what product would best be used to attach the carbon post and alloy head. Thank in advance. Stephen
|
By scottracing - 12/29/2019 6:28:35 PM
can you post a picture? I would clean and inspect both parts to ensure there is no damage or delamination.
Ive used DP490 to great effect on the bike frames ive built,but you need to ensure that your bonding surfaces are properly abraded and clean.
|
|