By Shaneer22 - 11/18/2012 10:55:28 PM

Hi I've been looking on here for a while,some good info,Iam modifying my bike into a track focused bike,started today on making the pattern,alot off on off carving far from finished,spent about 1 hour so far really easy to shape the foam,which was a great help,the idea is to lower centre of gravity on the bike.i will post photo's at each stage of the build,any suggestion comments welcome. webkit-fake-url://57A9E304-474C-4E00-BBA8-60A41B67D504/imagejpeg
By Shaneer22 - 11/19/2012 4:30:08 PM

Posted from iPad and for some reason not working I will do it from pc.