By Jones - 12/9/2019 5:51:45 PM
Hi! I’m reverting back to resin infusion again, I have in the past had a lot of troubles with resin infusion. Everything from banging and layup time to perfectly sealed bags: What is your favourite base materials such as: Banging film Tacky tape Epoxy Release system Digital vacuum gauge Peelply, perforated film, flow media etc. (Are three in one worth it for example) Basically what is your favourite tools and materials to use?
Im based in Europe, Sweden. The idea behind the thread is more so to see what materials people prefer and why.
|
By MarkMK - 12/11/2019 9:20:45 AM
It might be helpful to say where in the world you are, as some products might only be accessible in certain locations?
|
|