By Otolithco - 12/7/2019 2:21:17 AM
I am working on a complex part that is proving tough for infusion. I have used 3M adhesive sparingly on the mould for the first layer with good results. But the remaining layers are difficult to lay up.
Has anyone run into issues using adhesive between layers of carbon fiber?
|
By Pleochroic - 12/24/2019 10:47:58 PM
I had never encountered with after-stained with gorilla adhesive spray...
|
|