By arsentis arsentisgr - 10/18/2019 9:53:18 AM
Hello ! My name is Arsentis, I'm from Greece, I found your online store "www.easycomposites.co.uk" Please advise me which components I need to buy in order to cast marble - stone, I want to get as a result of a sculpture that will look like marble. I bought a silicone mold for casting a statue of the ancient Greek goddess 1.7 meter high, the article will be on the street , need weather resistance. I was told that it is better to make marble from : polyester resin , gelcoat , epoxy thickener , hardener for polyester resins - mix it all and pour it into my mold . And you have these components, or maybe you know some other recipe for pouring liquid marble - stone . Please tell me exactly which components and how much should I buy in order to fill in one statue first.. Thank . Arsentis .
|
By Yassine - 10/18/2019 3:29:21 PM
+xHello ! My name is Arsentis, I'm from Greece, I found your online store "www.easycomposites.co.uk" Please advise me which components I need to buy in order to cast marble - stone, I want to get as a result of a sculpture that will look like marble. I bought a silicone mold for casting a statue of the ancient Greek goddess 1.7 meter high, the article will be on the street , need weather resistance. I was told that it is better to make marble from : polyester resin , gelcoat , epoxy thickener , hardener for polyester resins - mix it all and pour it into my mold . And you have these components, or maybe you know some other recipe for pouring liquid marble - stone . Please tell me exactly which components and how much should I buy in order to fill in one statue first.. Thank . Arsentis . Hi dear,
Nice to see you are planning to cast liquid marble. Firstly, liquid marble made from gelcoat, polyester resin and limestone (calcium carbonat). They cost respectively (4$ to 6$), (1.5$ to 3$) and for limestone is inxpinsive and available evrywhere.
kind regards
|
|