+xHi. Yes I’ve seen the video and I’ve made a few tables. This one has been sanded down to 1500 grit then I’ve used the NW1 but I can’t get it clear enough and I still need to coat the wood so wondered if o could just paint on some resin
In theory you could, and this should bring this back up to full gloss but there is a potential of it not being completely smooth. I would suggest coating a small area, like a cut off first before moving onto the main project and see what the outcome would look like.
I am sorry i do not have better news for you.