By Skywalker - 10/8/2019 9:32:16 AM
Hi. I am starting a project at home which requires me to make a clear block of resin around 6 inches square with various items inside. Ive been looking at the GlassCast 50 Clear Epoxy Casting Resin. Is this suitable for this kind of project? It does state it can go 25mm deep so I guess multiple layers at 25mm?
|
By Warren (Staff) - 10/9/2019 2:14:53 PM
Yes the GlassCast 50 is the product you need.
|
|