By C Rolfe - 9/26/2019 8:44:48 AM
Hi there, I'm an art technician in an art department for a secondary school. Our A-Level students are looking to use some Epoxy resin, I was wondering if i could get any advice on a resin safe to use in schools and age appropriate?
|
By Warren (Staff) - 9/27/2019 3:29:42 PM
For that kind of work, casting up to 10mm per layer, then you can use the GlassCast 10 Clear Epoxy Casting Resin. If you pour each subsequent layer when the previous one has become firm but tacky (the B stage cure), then you will minimise the chance of seeing lines between each pour.
|
|