By debbie - 9/25/2019 10:32:45 AM				
            
                      
            Hi, I have ordered the rubber silicone to make a new mould for a damaged item. I’ve had a couple of unsuccessful attempts on glass but this is resin. If I pour a later into the base of a container and fill the space with rubber silicone will it peel away from the acrylic or do I need a release agent? Thanks
           
		 | 			
		 
	
		
				      		    
		
		
            
            
            By Hanaldo - 9/25/2019 11:28:17 PM				
            
                      
            Shouldn't need a release agent, silicone only really bonds to itself and glass (as glass contains silica). 
           
		 | 			
		 
	
	
						
		 	
		
	 |