By KimJa - 9/22/2019 5:52:07 PM				
            
                      
            Good day,  I hope you all are well. I am very new to mould making and am having a challenge. I want to make a silicone mould of a vase that is not straight up and down, it has curves and is hollow inside. I have done some research and seen how someone made a mould of a solid ball in two parts. I have been trying to wrap my head around how I would get this done for a vase with a hollow section bue have not come up with anything that looks practical. I a seeking your guidance, thanks in advance. I have attached two vases I am attempting to make a silicone mould from.
           
		 | 			
		 
	
		
				      		    
		
		
            
            
            By Warren (Staff) - 9/25/2019 8:43:44 AM				
            
                      
            yes. Something easy to remove to reduce the silicone volume and thus creating space to flex the silicone away from the casts surface once cured.
           
		 | 			
		 
	
	
						
		 	
		
	 |