By DavidMerch - 9/4/2019 8:31:03 PM

Hello
I would like to make a sandwich structure using two of your cured Carbon fiber panels 1.5mm thick. In the middle I plan to bond 10mm thick PMMA plastic, what glue do you suggest? Any surface preparation?
Can you also advise if other laser cut plastic are better for this purpose? The structure will be subjected to low loads.

Thanks
By Hanaldo - 9/6/2019 4:12:12 AM

Thoroughly sand the surface with 80 grit sandpaper, then clean with isopropyl alcohol.